Marl
USGS DS-801 XRD marl 36.4072, -105.5731
4-Acid ICP + Rietveld QXRD
ID: DS801-NM-012-C
DOI: 10.3133/ds801 ↗
Smith et al. (2013), USGS Data Series 801
SiO2
56.38%
Al2O3
12.55%
Fe₂O₃(T)
3.67%
CaO
10.04%
MgO
2.49%
K2O
2.51%
Na2O
1.63%
LOI
9.92%