Geochemical Inference, Petrology & Ceramic Melt Physics Methodology
DCI Tailor couples spheroidal PostGIS stratigraphy, Compositional Data Analysis (CoDA), pedogenic horizon priors, constrained non-negative least-squares (NNLS) normative mineralogy, and non-Arrhenian magmatic melt physics to translate field-collected clays, rocks, and ashes into quantitative ceramic chemistry. Every equation and reference constant below is evaluated live against 9 official USGS and NIST Certified Reference Materials (CRMs).
Stratigraphic Polygon Matching, Spatial Declustering & Compositional Data Analysis (CoDA)
Hierarchical PostGIS Tiered Search
Rather than pooling across fault contacts or batholith boundaries with isotropic circles first, BaselineEstimatorService evaluates:
- Tier 0 (Same-Polygon):
ST_Covers(ST_MakeValid(unit.boundary), location)with Quaternary surficial selection (t_age ≤ 2.58 Ma) forwild_clayvs. pre-Quaternary bedrock (b_age > 2.58 Ma) forcrushed_rock, ranked by Macrostrat compilation scale. - Tier 0b (Fluvial Basin): Upstream HUC-12 / USGS NLDI watershed polygon for floodplain alluvial clays.
- Tiers 1–3: 15 km and 50 km WGS84 spheroidal radii restricted to petrogenetically compatible rock families (never pooling felsic granite with calcitic limestone or ultramafic serpentinite).
Cell Declustering & Kish Effective Sample Size
Geochemical databases exhibit severe drillhole/quarry clustering. Specimens are declustered over 0.0025° (~275 m) spatial cells (wi = wsource · wlith · wIDW / ncell), and sample-count evidence is governed by Kish's (1965) effective sample size bounded by unique spatial cells C:
Heuristic scores are explicitly labeled Calibration Index (0–95%) alongside non-parametric IQR (P25–P75) bars, never conflated with frequentist 1 − α confidence intervals.
Aitchison (1986) Log-Ratio Simplex Center
Component-wise medians violate constant-sum closure (SD) and artificially zero-bias anhydrous microprobe/XRF rows. DCI Tailor replaces below-detection zeros via Martín-Fernández et al. (2003) multiplicative replacement (δ = 0.005 wt%) and computes weighted geometric centers on the 10-oxide volatile-free simplex:
Unmeasured anhydrous LOI rows are excluded from LOI* estimation so fresh igneous compilations never suppress clay structural water.
Silicate Weathering Indices, IUGS TAS Classification & Constrained NNLS Normative Mineralogy
CIA, PIA, ICV, WIP & McLennan CaO*
Molar oxide proportions quantify feldspar-to-kaolinite hydrolysis. Silicate CaO* subtracts fluorapatite ((10/3) P₂O₅) and applies McLennan's (1993) CaO* ≤ Na₂O cap when LOI ≥ 2.5 wt%:
Non-silicate carbonates/ashes, high-volatile kerogen marlstones, and low-Al₂O₃ ultramafics are explicitly gated so limestone, oil shale, or serpentinite is never misclassified as weathered kaolin or fresh feldspar.
IUGS TAS (Le Bas 1986) & Irvine–Baragar (1971)
Whole-rock igneous samples are normalized to a 100% volatile-free basis across all 15 official IUGS polygons with Middlemost (1994) plutonic equivalents and the exact 6th-order Irvine & Baragar (1971, Appendix II) magma-series divide (A = Na₂O + K₂O):
Dual-Mode NNLS Normative Solver
NormativeMineralogyService minimizes ‖W(Ax − b)‖22 subject to x ≥ 0:
- MINSQ Clay/Sediment Basis (Herrmann & Berry, 2002): Quartz, Kaolinite, Illite, Smectite, Chlorite, Albite, K-Feldspar, Anorthite, Calcite, Dolomite, Hematite, Anatase, Apatite (gating carbonates when
vinegar_fizz = none). - 3-Branch CIPW Igneous Basis (Cross et al., 1902): Evaluates mutually exclusive Quartz + Hypersthene + Corundum, Hypersthene + Olivine, and Olivine + Nepheline branches so neither
Q + OlnorNe + Hyever coexist.
Seger UMF, Kiln Redox Partitioning, Polymerization (NBO/T), VFT Melt Viscosity & Optical Basicity
Redox-Aware Seger UMF & Stull (1912)
Unity Molecular Formula normalizes Σ(R₂O + RO) = 1.000 against R₂O₃ intermediates and RO₂ + R₂O₅ network formers. In Cone 10 Reduction, 80% of molar Fe partitions into divalent FeO (RO fayalite flux) while 20% remains Fe₂O₃, shifting SiO₂ and Al₂O₃ UMF coordinates on the Stull (1912) diagram.
Mysen (1988) NBO/T, Giordano VFT & Angell Fragility m
MeltPhysicsService computes Non-Bridging Oxygens per Tetrahedron after charge-balancing tetrahedral AlIV, Fe3+,IV, and Dell–Bray–Xiao BIV against Qmod = nM+ + 2nM2+, and evaluates Giordano, Russell & Dingwell (2008, Table 1) non-Arrhenian melt viscosity plus Angell (1995) kinetic fragility m = B·Tg / (Tg − C)²:
Optical Basicity Λ & Linear COE
Oxygen-equivalent weighted Duffy & Ingram (1976) optical basicity (Λ = Σ ni zO,i Λi / Σ ni zO,i) predicts transition-metal (Fe, Cu, Co, Mn) valence/coordination color shifts, while English–Turner / Mayer–Havas factors predict linear glaze thermal expansion in × 10−6 /°C (ppm/K).
Whole-Rock Analytical QA/QC, Negative Mafic LOI & Mineralogical/ED-XRF Hazard Screening
Washington (1917) / Rollinson (1993) Closure & Ferrous LOI
Pre-normalization lab XRF totals are audited against the standard 98.0–101.5 wt% acceptance window before 100% closure, avoiding FeOT/Fe₂O₃* double-counting and permitting negative gravimetric LOI ∈ [-2.5%, 0%) on fresh ferrous basalts (2FeO + ½O₂ → Fe₂O₃, +0.11135 wt% oxygen gain; Lechler & Desilets, 1987). USGS DS-801 4-acid ICP analyses reconstruct volatilized SiF₄↑ silica from Rietveld QXRD mineral stoichiometries (including amorphous volcanic glass).
Toxic Trace, NORM, Fibrous Silicate & pXRF Line-Overlap Screening
HazardScreenerService screens toxic heavy metals (Pb, Cd, As, Ba, Cr, Mn, V), pegmatite Beryllium (Be ≥ 15 ppm / beryl), asbestiform amphiboles/serpentines/erionite, secular-equilibrium radioactivity (Aeq = U/81 + Th/246 Bq/g), LCT pegmatite K/Rb < 160 lithium pathfinders, and handheld ED-pXRF spectral interferences (Pb Lα/As Kα, Ba Lα/Ti Kα, Ti Kβ/V Kα, Rb Kα/U Lα).
USGS & NIST Certified Reference Material (CRM) Validation Matrix (9 Standards)
Computed dynamically on every request from published USGS and NIST Certificates of Analysis — zero hardcoded output values. Click Load in Workbench on any standard to inspect its full Stull, TAS, A–CN–K, normative, and blend behavior.
| Standard & Locality | Raw Sum | IUGS TAS / CIA | Dominant Normative Assemblage | UMF Si:Al | NBO/T · ηΔ10 · Λ | Workbench |
|---|---|---|---|---|---|---|
|
USGS BHVO-2 · Hawaiian Volcanic Observatory Basalt
Halemaʻumaʻu 1919 Pāhoehoe Flow, Kīlauea, Hawaiʻi
Archetypal ocean-island tholeiitic basalt (<52 wt% SiO₂) plotting squarely in Subalkaline Basalt (B) with fluid Cone 10 melt viscosity (~1.5 log₁₀ Pa·s).
|
100.24% |
Basalt
Subalkaline · CIA 35.7
|
Diopside (Cpx) 27.8%, Anorthite (An) 19.0%, Albite (Ab) 18.7%
CIPW · RMSD 0.02%
|
6.27:1
COE 7.04
|
NBO/T 0.34 · m 46.9
η₁₀ 1.27 · Λ 0.57
|
|
|
USGS BCR-2 · Columbia River Basalt (Bridal Veil Flow)
Bridal Veil Flow Quarry, Columbia River Gorge, Oregon
Evolved Grande Ronde flood basalt (54.1% SiO₂ > 52.0% IUGS boundary): classic petrology benchmark plotting in Subalkaline Basaltic Andesite (O1) with quartz-hypersthene CIPW norm; prime PNW single-rock tenmoku/iron glaze.
|
99.87% |
Basaltic Andesite
Subalkaline · CIA 41.2
|
Albite (Ab) 26.7%, Diopside (Cpx) 19.3%, Quartz (Q) 14.7%
CIPW · RMSD 0.01%
|
6.80:1
COE 7.33
|
NBO/T 0.10 · m 38.8
η₁₀ 1.98 · Λ 0.55
|
|
|
USGS AGV-2 · Guano Valley Andesite (Trachyandesite)
Guano Valley Rim, Lake County, SE Oregon
Named petrographically by Flanagan (1967) prior to Le Bas et al. (1986); volatile-free Na₂O+K₂O = 7.17% at 60.15% SiO₂ crosses the 6.48% O2/S3 line into Subalkaline Trachyandesite (S3).
|
100.20% |
Trachyandesite
Subalkaline · CIA 48.0
|
Albite (Ab) 35.5%, Quartz (Q) 17.9%, Orthoclase (Or) 17.0%
CIPW · RMSD 0.00%
|
5.95:1
COE 7.08
|
NBO/T 0.04 · m 32.4
η₁₀ 2.91 · Λ 0.55
|
|
|
USGS GSP-2 · Silver Plume Granodiorite
Silver Plume Quarry, Clear Creek County, Colorado
Proterozoic high-K calc-alkaline granitoid (CIA = 52.4 ≈ Upper Continental Crust 52.8; 5.38% K₂O shifts anhydrous alkalis just across the Le Bas O3/T Quartz Monzonite boundary); monazite Th = 105 ppm triggers NORM screening.
|
100.15% |
Trachyte / Trachydacite
Subalkaline · CIA 52.4
|
Orthoclase (Or) 31.8%, Quartz (Q) 27.8%, Albite (Ab) 23.5%
CIPW · RMSD 0.01%
|
7.59:1
COE 6.63
|
NBO/T 0.00 · m 27.4
η₁₀ 3.84 · Λ 0.54
|
|
|
USGS RGM-2 · Glass Mountain Rhyolite Obsidian
Glass Mountain Flow, Medicine Lake Highland, Siskiyou Co., CA
Benchmark Subalkaline Rhyolite (R) with strong polymerized tectosilicate network (NBO/T ≈ 0.00, log₁₀ η ≈ 4.39 Pa·s at Cone 10, fragility m ≈ 24.7) requiring CaO/wood-ash RO fluxing.
|
100.00% |
Rhyolite
Subalkaline · CIA 50.7
|
Albite (Ab) 35.0%, Quartz (Q) 31.3%, Orthoclase (Or) 25.7%
CIPW · RMSD 0.00%
|
8.90:1
COE 6.18
|
NBO/T 0.00 · m 24.7
η₁₀ 4.39 · Λ 0.53
|
|
|
USGS SGR-1b · Green River Dolomitic Oil Shale
Mahogany Zone, Green River Formation, Piceance Basin, CO
Carbonate-kerogen marlstone validating McLennan (1993) CaO* <= Na₂O cap, normative dolomite reconstruction, and As + S kiln degassing hazard screening.
|
100.00% |
Non-Silicate / Carbonate
ICV 3.86
|
Dolomite 53.9%, Kaolinite 28.6%, Quartz (Free SiO₂) 13.1%
MINSQ · RMSD 5.55%
|
7.35:1
COE 8.69
|
NBO/T 0.76 · m 43.5
η₁₀ 1.07 · Λ 0.60
|
|
|
NIST SRM 70a · Potassium Feldspar (Perthitic Microcline)
Kingman Pegmatite District, Mohave County, Arizona
Monomineralic pegmatite potash-spar crystal separate (CIA = 51.1 vs stoichiometric feldspar 50.0; UMF 0.99 R₂O : 1.04 Al₂O₃ : 6.36 SiO₂; whole-rock volcanic TAS N/A).
|
99.96% |
Mineral Separate (K-Feldspar)
TAS N/A · CIA 51.0
|
Orthoclase (Or) 69.8%, Albite (Ab) 21.6%, Quartz (Q) 7.1%
CIPW · RMSD 0.07%
|
6.36:1
COE 8.01
|
NBO/T 0.00 · m 23.8
η₁₀ 4.35 · Λ 0.55
|
|
|
NIST SRM 97b · Flint Clay (Refractory Kaolinite)
Clearfield Pennsylvanian Underclay District, Pennsylvania
Extreme leached 1:1 kaolinitic end-member (CIA = 98.1, PIA = 99.7, ICV = 0.13, ~95% normative Kaolinite, Stull Unfused/Refractory, outside GRD08 magmatic liquidus).
|
99.61% |
CIA 98.0 · PIA 99.7
Intense Weathering · Kaolinitic Zone (CIA > 82) · ICV 0.13
|
Kaolinite 95.1%, Anatase / Rutile 2.4%, Hematite / Goethite 1.3%
MINSQ · RMSD 0.83%
|
1.83:1
COE 4.16
|
NBO/T 0.00
η₁₀ sub-liq · Λ 0.54
|
|
|
NIST SRM 679 · Brick Clay (Ferruginous Illite–Kaolinite)
Potomac Group Coastal Plain Clay, Maryland / D.C.
Classic red-firing terracotta / Cone 10 reduction slip clay (CIA = 85.7, ICV = 0.79 < 1.0 mature clay; 12.94% Fe₂O₃(T) shifts strongly into RO flux in reduction).
|
100.05% |
CIA 85.7 · PIA 98.3
Intense Weathering · Kaolinitic Zone (CIA > 82) · ICV 0.79
|
Kaolinite 31.7%, Quartz (Free SiO₂) 17.0%, Smectite 14.0%
MINSQ · RMSD 0.10%
|
4.25:1
COE 5.75
|
NBO/T 0.00
η₁₀ sub-liq · Λ 0.52
|
Primary Literature Citations & BibTeX Archive
@article{peters2018macrostrat,
author = {Peters, Shanan E. and Husson, Jon M. and Czaplewski, John},
title = {Macrostrat: A Platform for Geological Data Integration and Deep-Time Earth Crust Research},
journal = {Geochemistry, Geophysics, Geosystems},
year = {2018},
volume = {19},
number = {4},
pages = {1393--1409},
doi = {10.1029/2018GC007467}
}
@techreport{smith2013usgs_ds801,
author = {Smith, David B. and Cannon, William F. and Woodruff, Laurel G. and Solano, Federico and Kilburn, James E. and Fey, David L.},
title = {Geochemical and Mineralogical Data for Soils of the Conterminous {United States}},
institution = {U.S. Geological Survey},
type = {Data Series},
number = {801},
year = {2013},
doi = {10.3133/ds801}
}
@article{nesbitt1982cia,
author = {Nesbitt, H. W. and Young, G. M.},
title = {Early {Proterozoic} Climates and Plate Motions Inferred from Major Element Chemistry of Lutites},
journal = {Nature},
year = {1982},
volume = {299},
pages = {715--717},
doi = {10.1038/299715a0}
}
@article{mclennan1993weathering,
author = {McLennan, Scott M.},
title = {Weathering and Global Denudation},
journal = {The Journal of Geology},
year = {1993},
volume = {101},
number = {2},
pages = {295--303},
doi = {10.1086/648222}
}
@article{fedo1995unraveling,
author = {Fedo, Christopher M. and Nesbitt, H. Wayne and Young, Grant M.},
title = {Unraveling the Effects of Potassium Metasomatism in Sedimentary Rocks and Paleosols, with Implications for Paleoweathering Conditions and Provenance},
journal = {Geology},
year = {1995},
volume = {23},
number = {10},
pages = {921--924},
doi = {10.1130/0091-7613(1995)023<0921:UTEOPM>2.3.CO;2}
}
@article{cox1995influence,
author = {Cox, Randal and Lowe, Donald R. and Cullers, Robert L.},
title = {The Influence of Sediment Recycling and Basement Composition on Evolution of Mudrock Chemistry in the Southwestern {United States}},
journal = {Geochimica et Cosmochimica Acta},
year = {1995},
volume = {59},
number = {14},
pages = {2919--2940},
doi = {10.1016/0016-7037(95)00185-9}
}
@article{parker1970index,
author = {Parker, Andrew},
title = {An Index of Weathering for Silicate Rocks},
journal = {Geological Magazine},
year = {1970},
volume = {107},
number = {6},
pages = {501--504},
doi = {10.1017/S0016756800058581}
}
@article{middlemost1994naming,
author = {Middlemost, Eric A. K.},
title = {Naming Materials in the Magma/Igneous Rock System},
journal = {Earth-Science Reviews},
year = {1994},
volume = {37},
number = {3--4},
pages = {215--224},
doi = {10.1016/0012-8252(94)90029-9}
}
@article{winkler1954bedeutung,
author = {Winkler, Helmut G. F.},
title = {Bedeutung der Korngr{\"o}ssenverteilung und des Mineralbestandes von Tonen f{\"u}r die Herstellung grobkeramischer Erzeugnisse},
journal = {Berichte der Deutschen Keramischen Gesellschaft},
year = {1954},
volume = {31},
pages = {337--343}
}
@article{jochum2016georem,
author = {Jochum, Klaus Peter and Weis, Ulrike and Schwager, B{\"a}rbel and Stoll, Brigitte and Wilson, Stephen A. and Haug, Gerald H. and Andreae, Meinrat O. and Enzweiler, Jacinta},
title = {Reference Values Following {ISO} Guidelines for Frequently Requested Rock Reference Materials},
journal = {Geostandards and Geoanalytical Research},
year = {2016},
volume = {40},
number = {3},
pages = {333--350},
doi = {10.1111/ggr.12094}
}
@article{lebas1986tas,
author = {Le Bas, M. J. and Le Maitre, R. W. and Streckeisen, A. and Zanettin, B.},
title = {A Chemical Classification of Volcanic Rocks Based on the Total Alkali--Silica Diagram},
journal = {Journal of Petrology},
year = {1986},
volume = {27},
number = {3},
pages = {745--750},
doi = {10.1093/petrology/27.3.745}
}
@article{irvine1971chemical,
author = {Irvine, T. N. and Baragar, W. R. A.},
title = {A Guide to the Chemical Classification of the Common Volcanic Rocks},
journal = {Canadian Journal of Earth Sciences},
year = {1971},
volume = {8},
number = {5},
pages = {523--548},
doi = {10.1139/e71-055}
}
@book{aitchison1986coda,
author = {Aitchison, John},
title = {The Statistical Analysis of Compositional Data},
publisher = {Chapman and Hall},
address = {London},
year = {1986}
}
@article{martinferndez2003zeros,
author = {Mart{\'i}n-Fern{\'a}ndez, J. A. and Barcel{\'o}-Vidal, C. and Pawlowsky-Glahn, V.},
title = {Dealing with Zeros and Missing Values in Compositional Data Sets Using Nonparametric Imputation},
journal = {Mathematical Geology},
year = {2003},
volume = {35},
number = {3},
pages = {253--278},
doi = {10.1023/A:1023866030544}
}
@article{herrmann2002minsq,
author = {Herrmann, Walter and Berry, Ron F.},
title = {{MINSQ} --- A Least Squares Spreadsheet Method for Calculating Mineral Proportions from Whole Rock Major Element Analyses},
journal = {Geochemistry: Exploration, Environment, Analysis},
year = {2002},
volume = {2},
number = {4},
pages = {361--368},
doi = {10.1144/1467-787302-010}
}
@article{giordano2008viscosity,
author = {Giordano, Daniele and Russell, James K. and Dingwell, Donald B.},
title = {Viscosity of Magmatic Liquids: A Model},
journal = {Earth and Planetary Science Letters},
year = {2008},
volume = {271},
number = {1--4},
pages = {123--134},
doi = {10.1016/j.epsl.2008.03.038}
}
@article{angell1995formation,
author = {Angell, C. Austen},
title = {Formation of Glasses from Liquids and Biopolymers},
journal = {Science},
year = {1995},
volume = {267},
number = {5206},
pages = {1924--1935},
doi = {10.1126/science.267.5206.1924}
}
@book{mysen1988silicate,
author = {Mysen, Bjorn O.},
title = {Structure and Properties of Silicate Melts},
publisher = {Elsevier},
address = {Amsterdam},
year = {1988}
}
@article{duffy1976optical,
author = {Duffy, J. A. and Ingram, M. D.},
title = {An Interpretation of Glass Chemistry in Terms of the Optical Basicity Concept},
journal = {Journal of Non-Crystalline Solids},
year = {1976},
volume = {21},
number = {3},
pages = {373--410},
doi = {10.1016/0022-3093(76)90027-2}
}
@article{stull1912porcelain,
author = {Stull, Ray T.},
title = {Influences of Variable Silica and Alumina on Porcelain Glazes of Constant {RO}},
journal = {Transactions of the American Ceramic Society},
year = {1912},
volume = {14},
pages = {62--70}
}
@book{rollinson1993geochemical,
author = {Rollinson, Hugh R.},
title = {Using Geochemical Data: Evaluation, Presentation, Interpretation},
publisher = {Longman Scientific \& Technical},
year = {1993}
}