Staging copy — test data only (dci-tailor-staging.glazecalcapp.com)
SiO₂
DCI Tailor Spatial Atlas
Community Verified XRF/pXRF & Geological Reference Assays
Public Atlas Assays
62
Community Verified (2.5× Prior)
0
USGS / Academic Surveys
62
Mapped Lithologies
15
Regional Geochemical Map
Community XRF / pXRF USGS / Academic Survey

Marl

USGS DS-801 XRD marl 36.4072, -105.5731
4-Acid ICP + Rietveld QXRD ID: DS801-NM-012-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.38%
Al2O3
12.55%
Fe₂O₃(T)
3.67%
CaO
10.04%
MgO
2.49%
K2O
2.51%
Na2O
1.63%
LOI
9.92%

Alluvial Clay

USGS DS-801 XRD alluvial clay 40.6187, -80.5773
4-Acid ICP + Rietveld QXRD ID: DS801-OH-011-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.72%
Al2O3
20.16%
Fe₂O₃(T)
4.57%
CaO
0.66%
MgO
1.21%
K2O
2.78%
Na2O
0.42%
LOI
5.21%

Kaolin Clay

USGS DS-801 XRD kaolin clay 36.7417, -88.6367
4-Acid ICP + Rietveld QXRD ID: DS801-KY-010-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
61.06%
Al2O3
24.94%
Fe₂O₃(T)
2.04%
CaO
0.30%
MgO
0.52%
K2O
1.36%
Na2O
0.24%
LOI
8.00%

Glacial Clay

USGS DS-801 XRD glacial clay 42.0347, -93.6200
4-Acid ICP + Rietveld QXRD ID: DS801-IA-009-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
61.91%
Al2O3
11.90%
Fe₂O₃(T)
3.98%
CaO
7.11%
MgO
2.79%
K2O
1.98%
Na2O
1.29%
LOI
8.29%

Kaolin Clay

USGS DS-801 XRD kaolin clay 32.9815, -82.8101
4-Acid ICP + Rietveld QXRD ID: DS801-GA-008-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.52%
Al2O3
29.14%
Fe₂O₃(T)
1.91%
CaO
0.17%
MgO
0.26%
K2O
0.62%
Na2O
0.12%
LOI
9.63%

Alluvial Clay

USGS DS-801 XRD alluvial clay 45.7090, -121.5290
4-Acid ICP + Rietveld QXRD ID: DS801-OR-007-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
56.24%
Al2O3
16.74%
Fe₂O₃(T)
9.57%
CaO
4.25%
MgO
3.11%
K2O
1.07%
Na2O
2.49%
LOI
4.22%

Alluvial Clay

USGS DS-801 XRD alluvial clay 44.9429, -123.0351
4-Acid ICP + Rietveld QXRD ID: DS801-OR-006-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.10%
Al2O3
16.98%
Fe₂O₃(T)
6.66%
CaO
2.22%
MgO
1.88%
K2O
1.83%
Na2O
2.01%
LOI
4.02%

Loess

USGS DS-801 XRD loess 46.8450, -117.3620
4-Acid ICP + Rietveld QXRD ID: DS801-WA-005-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
68.15%
Al2O3
13.72%
Fe₂O₃(T)
4.92%
CaO
2.94%
MgO
1.82%
K2O
2.36%
Na2O
2.22%
LOI
2.75%

Kaolin Clay

USGS DS-801 XRD kaolin clay 47.5620, -117.1050
4-Acid ICP + Rietveld QXRD ID: DS801-WA-004-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
60.28%
Al2O3
25.32%
Fe₂O₃(T)
2.29%
CaO
0.57%
MgO
0.61%
K2O
2.87%
Na2O
0.89%
LOI
6.21%

Glacial Clay

USGS DS-801 XRD glacial clay 47.6120, -122.5340
4-Acid ICP + Rietveld QXRD ID: DS801-WA-003-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
60.92%
Al2O3
16.66%
Fe₂O₃(T)
6.44%
CaO
3.25%
MgO
2.65%
K2O
2.16%
Na2O
2.38%
LOI
4.42%

Alluvial Clay

USGS DS-801 XRD alluvial clay 47.1910, -122.2980
4-Acid ICP + Rietveld QXRD ID: DS801-WA-002-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
64.66%
Al2O3
15.98%
Fe₂O₃(T)
5.74%
CaO
2.64%
MgO
2.00%
K2O
2.03%
Na2O
2.45%
LOI
3.48%

Glacial Clay

USGS DS-801 XRD glacial clay 47.2580, -122.4520
4-Acid ICP + Rietveld QXRD ID: DS801-WA-001-C DOI: 10.3133/ds801 ↗ Smith et al. (2013), USGS Data Series 801
SiO2
63.90%
Al2O3
15.59%
Fe₂O₃(T)
6.07%
CaO
2.94%
MgO
2.30%
K2O
1.91%
Na2O
2.57%
LOI
3.67%

Sandersville Georgia GA

USGS NGDB kaolin clay 32.9815, -82.8101
Unit: Huber Formation Kaolin WD-XRF / ICP ID: USGS-PNW-050 USGS National Geochemical Database (NGDB)
SiO2
45.60%
Al2O3
38.40%
Fe₂O₃(T)
0.55%
CaO
0.12%
MgO
0.15%
K2O
0.20%
Na2O
0.08%
LOI
13.39%

Helena Montana MT

USGS NGDB limestone 46.5891, -112.0391
Unit: Madison Group Limestone WD-XRF / ICP ID: USGS-PNW-049 USGS National Geochemical Database (NGDB)
SiO2
6.10%
Al2O3
1.65%
Fe₂O₃(T)
0.70%
CaO
50.15%
MgO
1.45%
K2O
0.28%
Na2O
0.18%
LOI
39.29%

Madison Plateau Yellowstone WY

USGS NGDB rhyolite 44.6420, -110.8610
Unit: Lava Creek Rhyolite WD-XRF / ICP ID: USGS-PNW-048 USGS National Geochemical Database (NGDB)
SiO2
75.10%
Al2O3
12.60%
Fe₂O₃(T)
1.85%
CaO
0.75%
MgO
0.15%
K2O
5.20%
Na2O
3.50%
LOI
0.59%

Yosemite Sierra Nevada CA

USGS NGDB granite 37.7459, -119.5332
Unit: Half Dome Granitic Suite WD-XRF / ICP ID: USGS-PNW-047 USGS National Geochemical Database (NGDB)
SiO2
70.95%
Al2O3
14.85%
Fe₂O₃(T)
2.40%
CaO
2.25%
MgO
0.75%
K2O
4.15%
Na2O
3.75%
LOI
0.42%

McCall Idaho Batholith ID

USGS NGDB granite 44.9110, -116.0987
Unit: Atlanta Lobe Granite WD-XRF / ICP ID: USGS-PNW-046 USGS National Geochemical Database (NGDB)
SiO2
71.80%
Al2O3
14.60%
Fe₂O₃(T)
2.05%
CaO
1.85%
MgO
0.60%
K2O
4.60%
Na2O
3.65%
LOI
0.45%

Astoria Coast Range OR

USGS NGDB siltstone 46.1879, -123.8313
Unit: Astoria Formation Siltstone WD-XRF / ICP ID: USGS-PNW-045 USGS National Geochemical Database (NGDB)
SiO2
64.10%
Al2O3
15.95%
Fe₂O₃(T)
5.60%
CaO
2.75%
MgO
2.05%
K2O
2.10%
Na2O
2.30%
LOI
4.06%

Willamette Valley Salem OR

USGS NGDB siltstone 44.9429, -123.0351
Unit: Eugene Formation Siltstone WD-XRF / ICP ID: USGS-PNW-044 USGS National Geochemical Database (NGDB)
SiO2
65.20%
Al2O3
15.60%
Fe₂O₃(T)
5.15%
CaO
2.40%
MgO
1.80%
K2O
2.20%
Na2O
2.45%
LOI
4.18%

Klamath Mountains OR

USGS NGDB gabbro 42.2730, -123.6620
Unit: Josephine Ophiolite Gabbro WD-XRF / ICP ID: USGS-PNW-043 USGS National Geochemical Database (NGDB)
SiO2
49.40%
Al2O3
16.15%
Fe₂O₃(T)
9.50%
CaO
11.20%
MgO
8.10%
K2O
0.30%
Na2O
2.30%
LOI
1.64%

Fidalgo Island Anacortes WA

USGS NGDB gabbro 48.4850, -122.6420
Unit: Fidalgo Ophiolite Gabbro WD-XRF / ICP ID: USGS-PNW-042 USGS National Geochemical Database (NGDB)
SiO2
48.65%
Al2O3
16.40%
Fe₂O₃(T)
9.85%
CaO
11.45%
MgO
7.90%
K2O
0.35%
Na2O
2.20%
LOI
1.67%

Olympic Peninsula WA

USGS NGDB gabbro 47.9210, -123.5120
Unit: Crescent Formation Gabbro WD-XRF / ICP ID: USGS-PNW-041 USGS National Geochemical Database (NGDB)
SiO2
49.10%
Al2O3
15.80%
Fe₂O₃(T)
10.65%
CaO
10.90%
MgO
7.45%
K2O
0.45%
Na2O
2.45%
LOI
1.38%

Troy Latah County ID

USGS NGDB kaolin clay 46.7379, -116.7696
Unit: Bovill-Troy Kaolin WD-XRF / ICP ID: USGS-PNW-040 USGS National Geochemical Database (NGDB)
SiO2
48.50%
Al2O3
35.10%
Fe₂O₃(T)
0.95%
CaO
0.22%
MgO
0.28%
K2O
0.85%
Na2O
0.20%
LOI
12.84%

Freeman Spokane Basin WA

USGS NGDB kaolin clay 47.5150, -117.1940
Unit: Freeman Residual Kaolin WD-XRF / ICP ID: USGS-PNW-039 USGS National Geochemical Database (NGDB)
SiO2
49.20%
Al2O3
34.40%
Fe₂O₃(T)
1.25%
CaO
0.30%
MgO
0.35%
K2O
0.95%
Na2O
0.22%
LOI
12.14%

Mica Peak Spokane WA

USGS NGDB kaolin clay 47.5580, -117.0780
Unit: Latah Kaolin Deposit WD-XRF / ICP ID: USGS-PNW-038 USGS National Geochemical Database (NGDB)
SiO2
47.80%
Al2O3
35.60%
Fe₂O₃(T)
1.05%
CaO
0.25%
MgO
0.30%
K2O
0.75%
Na2O
0.18%
LOI
12.82%

Crater Lake OR

USGS NGDB rhyolite 42.9446, -122.1090
Unit: Cleekwood Rhyodacite WD-XRF / ICP ID: USGS-PNW-037 USGS National Geochemical Database (NGDB)
SiO2
71.40%
Al2O3
14.65%
Fe₂O₃(T)
2.65%
CaO
1.95%
MgO
0.55%
K2O
3.15%
Na2O
4.70%
LOI
0.45%

Newberry Caldera OR

USGS NGDB rhyolite 43.6880, -121.2390
Unit: Big Obsidian Flow WD-XRF / ICP ID: USGS-PNW-036 USGS National Geochemical Database (NGDB)
SiO2
73.20%
Al2O3
13.95%
Fe₂O₃(T)
2.10%
CaO
1.15%
MgO
0.25%
K2O
4.05%
Na2O
4.55%
LOI
0.42%

Bend Deschutes OR

USGS NGDB basalt 44.0582, -121.3153
Unit: High Cascades Basalt WD-XRF / ICP ID: USGS-PNW-035 USGS National Geochemical Database (NGDB)
SiO2
50.45%
Al2O3
16.10%
Fe₂O₃(T)
10.90%
CaO
9.50%
MgO
6.40%
K2O
0.85%
Na2O
3.05%
LOI
0.60%

Hood River Gorge OR

USGS NGDB basalt 45.7054, -121.5215
Unit: Columbia River Basalt WD-XRF / ICP ID: USGS-PNW-034 USGS National Geochemical Database (NGDB)
SiO2
52.10%
Al2O3
14.05%
Fe₂O₃(T)
12.85%
CaO
8.40%
MgO
4.80%
K2O
1.15%
Na2O
2.85%
LOI
1.01%

Yakima River Canyon WA

USGS NGDB basalt 46.8190, -120.4530
Unit: Roza Member Basalt WD-XRF / ICP ID: USGS-PNW-033 USGS National Geochemical Database (NGDB)
SiO2
50.85%
Al2O3
13.60%
Fe₂O₃(T)
14.15%
CaO
8.60%
MgO
4.55%
K2O
1.30%
Na2O
2.75%
LOI
0.77%

Pullman Palouse WA

USGS NGDB basalt 46.7313, -117.1796
Unit: Grande Ronde Basalt WD-XRF / ICP ID: USGS-PNW-032 USGS National Geochemical Database (NGDB)
SiO2
53.40%
Al2O3
14.20%
Fe₂O₃(T)
12.10%
CaO
8.10%
MgO
4.35%
K2O
1.40%
Na2O
2.95%
LOI
1.00%

Vantage Columbia River WA

USGS NGDB basalt 46.9445, -119.9870
Unit: Wanapum Basalt WD-XRF / ICP ID: USGS-PNW-031 USGS National Geochemical Database (NGDB)
SiO2
51.20%
Al2O3
13.85%
Fe₂O₃(T)
13.60%
CaO
8.75%
MgO
4.65%
K2O
1.25%
Na2O
2.80%
LOI
0.81%

Mount Baker Kulshan WA

USGS NGDB andesite 48.7767, -121.8144
Unit: Black Buttes Andesite WD-XRF / ICP ID: USGS-PNW-030 USGS National Geochemical Database (NGDB)
SiO2
59.85%
Al2O3
17.05%
Fe₂O₃(T)
6.45%
CaO
6.20%
MgO
3.25%
K2O
1.65%
Na2O
3.70%
LOI
0.62%

Mount St Helens WA

USGS NGDB andesite 46.2004, -122.1890
Unit: Spirit Lake Andesite WD-XRF / ICP ID: USGS-PNW-029 USGS National Geochemical Database (NGDB)
SiO2
62.35%
Al2O3
17.20%
Fe₂O₃(T)
5.30%
CaO
5.45%
MgO
2.30%
K2O
1.35%
Na2O
4.35%
LOI
0.70%

Paradise Mount Rainier WA

USGS NGDB andesite 46.7860, -121.7350
Unit: Mount Rainier Andesite WD-XRF / ICP ID: USGS-PNW-028 USGS National Geochemical Database (NGDB)
SiO2
61.10%
Al2O3
16.80%
Fe₂O₃(T)
6.10%
CaO
5.80%
MgO
2.85%
K2O
1.75%
Na2O
3.95%
LOI
0.53%

North Cascades Marblemount WA

USGS NGDB granite 48.4960, -121.1850
Unit: Cascade Pass Granite WD-XRF / ICP ID: USGS-PNW-027 USGS National Geochemical Database (NGDB)
SiO2
72.40%
Al2O3
14.30%
Fe₂O₃(T)
2.15%
CaO
1.65%
MgO
0.55%
K2O
4.45%
Na2O
3.70%
LOI
0.38%

Index Skykomish WA

USGS NGDB granodiorite 47.8206, -121.5551
Unit: Index Batholith WD-XRF / ICP ID: USGS-PNW-026 USGS National Geochemical Database (NGDB)
SiO2
66.45%
Al2O3
15.65%
Fe₂O₃(T)
4.20%
CaO
3.95%
MgO
1.70%
K2O
2.85%
Na2O
3.90%
LOI
0.53%

Snoqualmie Pass WA

USGS NGDB granodiorite 47.4240, -121.4137
Unit: Snoqualmie Batholith WD-XRF / ICP ID: USGS-PNW-025 USGS National Geochemical Database (NGDB)
SiO2
65.80%
Al2O3
15.90%
Fe₂O₃(T)
4.45%
CaO
4.15%
MgO
1.85%
K2O
2.75%
Na2O
3.80%
LOI
0.48%

Concrete Baker River WA

USGS NGDB limestone 48.5390, -121.7470
Unit: Chilliwack Limestone WD-XRF / ICP ID: USGS-PNW-024 USGS National Geochemical Database (NGDB)
SiO2
7.40%
Al2O3
1.95%
Fe₂O₃(T)
0.85%
CaO
48.90%
MgO
1.60%
K2O
0.35%
Na2O
0.20%
LOI
38.52%

Roche Harbor San Juan Island WA

USGS NGDB limestone 48.6095, -123.1510
Unit: Orcas Limestone WD-XRF / ICP ID: USGS-PNW-023 USGS National Geochemical Database (NGDB)
SiO2
5.20%
Al2O3
1.45%
Fe₂O₃(T)
0.65%
CaO
50.80%
MgO
1.25%
K2O
0.22%
Na2O
0.15%
LOI
40.10%

Chuckanut Drive Bellingham WA

USGS NGDB shale 48.6601, -122.4875
Unit: Chuckanut Formation Shale WD-XRF / ICP ID: USGS-PNW-022 USGS National Geochemical Database (NGDB)
SiO2
63.10%
Al2O3
18.20%
Fe₂O₃(T)
5.35%
CaO
1.40%
MgO
1.75%
K2O
2.85%
Na2O
1.60%
LOI
4.63%

Coupeville Whidbey Island WA

USGS NGDB marine clay 48.2189, -122.6860
Unit: Partridge Point Clay WD-XRF / ICP ID: USGS-PNW-021 USGS National Geochemical Database (NGDB)
SiO2
55.40%
Al2O3
18.05%
Fe₂O₃(T)
7.20%
CaO
4.50%
MgO
3.20%
K2O
2.35%
Na2O
2.55%
LOI
5.53%

Skagit Valley Burlington WA

USGS NGDB glacial clay 48.4712, -122.3254
Unit: Everson Glaciomarine Clay WD-XRF / ICP ID: USGS-PNW-020 USGS National Geochemical Database (NGDB)
SiO2
57.10%
Al2O3
17.95%
Fe₂O₃(T)
6.90%
CaO
3.60%
MgO
3.05%
K2O
2.40%
Na2O
2.30%
LOI
5.54%

Snohomish River Valley WA

USGS NGDB alluvial clay 47.9129, -122.0982
Unit: Snohomish Alluvium WD-XRF / ICP ID: USGS-PNW-019 USGS National Geochemical Database (NGDB)
SiO2
59.10%
Al2O3
16.85%
Fe₂O₃(T)
6.05%
CaO
2.95%
MgO
2.25%
K2O
2.20%
Na2O
2.45%
LOI
7.05%

Orting Carbon River WA

USGS NGDB andesite 47.0979, -122.2035
Unit: Mount Rainier Lahar Andesite WD-XRF / ICP ID: USGS-PNW-018 USGS National Geochemical Database (NGDB)
SiO2
60.20%
Al2O3
16.95%
Fe₂O₃(T)
6.40%
CaO
6.10%
MgO
2.95%
K2O
1.55%
Na2O
3.85%
LOI
0.84%

Tiger Mountain Issaquah WA

USGS NGDB siltstone 47.5005, -121.9760
Unit: Renton Siltstone WD-XRF / ICP ID: USGS-PNW-017 USGS National Geochemical Database (NGDB)
SiO2
66.40%
Al2O3
15.20%
Fe₂O₃(T)
4.85%
CaO
1.90%
MgO
1.60%
K2O
2.55%
Na2O
2.35%
LOI
4.20%

Enumclaw Plateau WA

USGS NGDB andesite 47.2043, -121.9915
Unit: Ohanapecosh Andesite WD-XRF / ICP ID: USGS-PNW-016 USGS National Geochemical Database (NGDB)
SiO2
59.40%
Al2O3
17.10%
Fe₂O₃(T)
6.80%
CaO
6.35%
MgO
3.15%
K2O
1.45%
Na2O
3.75%
LOI
0.78%

Olympia Budd Inlet WA

USGS NGDB glacial clay 47.0379, -122.9007
Unit: Olympia Beds WD-XRF / ICP ID: USGS-PNW-015 USGS National Geochemical Database (NGDB)
SiO2
58.75%
Al2O3
17.15%
Fe₂O₃(T)
6.50%
CaO
3.20%
MgO
2.55%
K2O
2.25%
Na2O
2.40%
LOI
6.08%

Nisqually Delta Lacey WA

USGS NGDB marine clay 47.0810, -122.7040
Unit: Puget Glaciomarine Drift WD-XRF / ICP ID: USGS-PNW-014 USGS National Geochemical Database (NGDB)
SiO2
56.20%
Al2O3
17.60%
Fe₂O₃(T)
6.80%
CaO
4.35%
MgO
2.90%
K2O
2.30%
Na2O
2.60%
LOI
6.08%

Black Diamond Green River Gorge WA

USGS NGDB shale 47.3087, -122.0032
Unit: Franklin Shale WD-XRF / ICP ID: USGS-PNW-013 USGS National Geochemical Database (NGDB)
SiO2
61.80%
Al2O3
19.40%
Fe₂O₃(T)
5.55%
CaO
1.10%
MgO
1.55%
K2O
3.10%
Na2O
1.30%
LOI
5.02%

Renton Cedar River WA

USGS NGDB shale 47.4829, -122.2171
Unit: Puget Group Shale WD-XRF / ICP ID: USGS-PNW-012 USGS National Geochemical Database (NGDB)
SiO2
62.50%
Al2O3
18.90%
Fe₂O₃(T)
5.20%
CaO
1.25%
MgO
1.65%
K2O
2.95%
Na2O
1.45%
LOI
4.95%

Duwamish Waterway Seattle WA

USGS NGDB alluvial clay 47.5280, -122.3200
Unit: Duwamish Deltaic Clay WD-XRF / ICP ID: USGS-PNW-011 USGS National Geochemical Database (NGDB)
SiO2
57.95%
Al2O3
16.90%
Fe₂O₃(T)
6.25%
CaO
3.40%
MgO
2.35%
K2O
2.05%
Na2O
2.75%
LOI
7.18%

West Seattle Alki Bluff WA

USGS NGDB marine clay 47.5750, -122.4050
Unit: Lawton Clay WD-XRF / ICP ID: USGS-PNW-010 USGS National Geochemical Database (NGDB)
SiO2
56.40%
Al2O3
18.25%
Fe₂O₃(T)
7.05%
CaO
3.85%
MgO
3.10%
K2O
2.55%
Na2O
2.50%
LOI
5.09%

Bainbridge Island WA

USGS NGDB marine clay 47.6262, -122.5212
Unit: Whidbey Marine Clay WD-XRF / ICP ID: USGS-PNW-009 USGS National Geochemical Database (NGDB)
SiO2
55.90%
Al2O3
17.85%
Fe₂O₃(T)
6.95%
CaO
4.10%
MgO
3.05%
K2O
2.40%
Na2O
2.65%
LOI
5.91%

Bremerton Kitsap WA

USGS NGDB glacial clay 47.5673, -122.6326
Unit: Kitsap Formation WD-XRF / ICP ID: USGS-PNW-008 USGS National Geochemical Database (NGDB)
SiO2
56.80%
Al2O3
18.45%
Fe₂O₃(T)
7.10%
CaO
2.80%
MgO
2.95%
K2O
2.35%
Na2O
2.10%
LOI
6.23%

Des Moines Bluff WA

USGS NGDB glacial clay 47.3850, -122.3450
Unit: Pre-Vashon Glacial Clay WD-XRF / ICP ID: USGS-PNW-007 USGS National Geochemical Database (NGDB)
SiO2
59.30%
Al2O3
17.40%
Fe₂O₃(T)
6.30%
CaO
3.15%
MgO
2.60%
K2O
2.20%
Na2O
2.35%
LOI
5.57%

Kent Valley WA

USGS NGDB alluvial clay 47.3809, -122.2348
Unit: White River Alluvium WD-XRF / ICP ID: USGS-PNW-006 USGS National Geochemical Database (NGDB)
SiO2
58.90%
Al2O3
17.05%
Fe₂O₃(T)
6.15%
CaO
2.90%
MgO
2.15%
K2O
2.10%
Na2O
2.40%
LOI
7.20%

Auburn Green River WA

USGS NGDB alluvial clay 47.3073, -122.2285
Unit: Green River Alluvium WD-XRF / ICP ID: USGS-PNW-005 USGS National Geochemical Database (NGDB)
SiO2
61.20%
Al2O3
16.10%
Fe₂O₃(T)
5.40%
CaO
2.70%
MgO
1.95%
K2O
2.25%
Na2O
2.50%
LOI
6.87%

Dash Point Federal Way WA

USGS NGDB glacial clay 47.3223, -122.4126
Unit: Lawton Clay Member WD-XRF / ICP ID: USGS-PNW-004 USGS National Geochemical Database (NGDB)
SiO2
57.60%
Al2O3
18.10%
Fe₂O₃(T)
6.85%
CaO
2.95%
MgO
2.80%
K2O
2.45%
Na2O
2.20%
LOI
5.85%

Gig Harbor Peninsula WA

USGS NGDB glacial clay 47.3293, -122.5801
Unit: Vashon Glacial Till WD-XRF / ICP ID: USGS-PNW-003 USGS National Geochemical Database (NGDB)
SiO2
60.15%
Al2O3
16.80%
Fe₂O₃(T)
6.10%
CaO
3.25%
MgO
2.50%
K2O
2.05%
Na2O
2.55%
LOI
5.47%

Puyallup Valley WA

USGS NGDB alluvial clay 47.1854, -122.2929
Unit: Holocene Alluvium WD-XRF / ICP ID: USGS-PNW-002 USGS National Geochemical Database (NGDB)
SiO2
59.80%
Al2O3
16.50%
Fe₂O₃(T)
5.90%
CaO
2.85%
MgO
2.20%
K2O
2.15%
Na2O
2.60%
LOI
6.90%

Tacoma Commencement Bay WA

USGS NGDB glacial clay 47.2740, -122.4680
Unit: Vashon Drift WD-XRF / ICP ID: USGS-PNW-001 USGS National Geochemical Database (NGDB)
SiO2
58.40%
Al2O3
17.20%
Fe₂O₃(T)
6.45%
CaO
3.10%
MgO
2.65%
K2O
2.30%
Na2O
2.45%
LOI
6.34%